Introduction
Garlock Helicoflex Metal O-Rings are designed to provide a high sealing level under adverse working conditions whether the medium is gas or liquid. Metal O-Rings are manufactured from stainless steel or high temperature alloy tubing or wire.
Sealing Concept
The sealing concept of Metal O-Rings is based on the elastic deformation of the tube which, during the compression cycle, gives a contact point on each sealing surface.
The tube characteristics determine the compressive load of the seal. This load combined with an accurate compression rate results in a specific pressure which is directly related to the sealing level obtained. A certain specific pressure is necessary to make the seal flow into the flange imperfections. A softer surface treatment is available to increase the plasticity of the seal and reduce the specific pressure necessary to reach the desired sealing level.
Metal O-Rings require a controlled compression by some mechanical method such as a custom machined groove or a limiter of appropriate thickness.
General Characteristics
Wide range of applications:
- Dimensional: Diameters from 0.250 inches (6.3 mm) to 300 inches (7.6 m)
- Cross sections from 0.031 inches (0.8 mm) to 0.625 inches (15.9 mm)
- Temperature: Cryogenic to 1800°F (982°C)
- Pressure: Ultra High Vacuum to 60000 PSI (4100 bar) Excellent springback Adaptable to a majority of standard flanges Available in many shape configurations: rectangular, oval, oblong etc... Suited to different types of assemblies: -metal/metal with groove
- flat flanges with a retainer
- 3 face contact Extended shelf life Excellent resistance to corrosion and radiation Minimum relaxation
Materials
Garlock Helicoflex Metal O-Rings can be manufactured using different materials such as 300 series Stainless Steel, Alloy 600, Alloy X750 or other special alloys. Temperature, pressure and corrosive aspects of the media determine which material is best suited for the application.
Heat Treatment
Since tensile strength and resilience of the seal are determined in part by metal temper, Garlock Helicoflex offers a choice of heat treatment (age hardening or annealing) according to AMS, MIL, ASTM or customer specification.
Plating / Coating
Sealing capability can be improved by platings or coatings such as Teflon®, silver, nickel or other malleable metals. These specialized surface treatments are recommended when sealing gaseous media. The coating or plating increases the seal plasticity and yields during installation, filling minor surface imperfections and creating a positive seal.
When service conditions allow, silver is the preferred surface treatment.
Different types of Seals
PLAIN Type : NP - The plain seal type NP (Not self energized or Pressure filled) is made of metal tubing (or wire) available in most metal alloys. This type is the most economical O-Ring. It is designed for low to moderate pressure and vacuum applications. |
|
SELF-ENERGIZING Type : SE - The surface exposed to the highest pressure, usually the inner periphery, is vented by small holes or slots. Self-Energizing seal type SE is recommended for high pressure applications. This feature allows the system pressure to enter the O-Rings, creating maximum specific pressure and reducing the pressure differential across the seal. For media other than high viscosity, one hole is sufficient. |
|
PRESSURE FILLED Type : PF - Pressure Filled O-Rings are designed for a temperature range of 800 to 2000°F (425-1093°C). The rings are filled with an inert gas at 600 PSI (41 bar). At elevated temperatures, gas pressure increases to offset the loss of strength in the tubing and specific pressure. |
O-Ring type Selection
TYPE NP : for working conditions from vacuum to 100 PSI (7 bar) TYPE SE : for pressure above 100 PSI (7 bar) and temperature up to 1800°F (982°C) TYPE PF : for high pressure and high temperature from 800°F (426°C) to 2000°F (1093°C)
Material Selection
Temperature and media to be sealed determine the type of O-Ring material
Temperature | O-Ring Material |
Cryogenic to 700°F (371°C) | Stainless Steel 321 |
Cryogenic to 1000°F (538°C) | Alloy 600 |
Cryogenic to 1400°F (760°C) | Alloy X750 |
Above 1400°F (760°C) | Consult our engineering staff |
O-Ring Size Selection
Tubing diameter is determined by ring outside diameter, available space and sealing level required. (see table on page 6) For each cross section, we have selected 3 different wall thicknesses. Thin (T), Medium (M) and Heavy (H), which give the appropriate specific pressure according to the required sealing level. (See table on page 5).
Plating / Coating
Different coatings or platings are available to provide better plasticity which yields and conforms to the microscopic groove or flange irregularities. The recommended surface treatments are :
Plating / Coating | Temperature |
Teflon® | Cryogenic to 500°F (260°C) |
Silver | Cryogenic to 1200°F (649°C) |
Nickel | Cryogenic to 2200°F (1204°C) |
Surface Finish Requirements
Plating / Coating | None | Teflon® | Silver | Nickel |
Recommended Surface Finish | <16 RMS | 16 To 32 RMS | 16 To 63 RMS | 16 To 32 RMS |
Ra in μm | <0.4 | 0.4 To 0.8 | 0.4 To 1.6 | 0.4 To 0.8 |
Specifications
The sealing level has been determined through intensive tests. : Low sealing Level Q > 10-5 Torr.liters.s-1 : Bubble Sealing Level 10-9 < Q < 10-5 Torr.Liters.s-1 : Helium Sealing Level Q < 10-9 Torr.Liters.s-1 Q : leak rate T : Thin M : Medium H : Heavy
Y2 : Ideal Compressive Load
e2 : Ideal Compression
Load characteristics change with wall thickness and material. We have selected 3 thicknesses : Thin(T), Medium(M), Heavy(H). The linear compressive load also depends on the material and the diameter of the seal. If we consider Y2* as the linear load for Stainless Steel 321, Km as material factor and Kd as diameter factor, the linear load Y2, under e2 will be :
Y2 = Km x Kd x Y2*
CS (Cross Section) = Tube Diameter
Standard Tubing | |||||||
Cross Section C.S. | Wall Thickness | ||||||
Thin | Medium | Heavy | |||||
in | mm | in | mm | in | mm | in | mm |
0.035 | 0.9 | 0.006 | 0.15 | 0.010 | 0.25 | N/A | N/A |
0.063 | 1.6 | 0.010 | 0.25 | 0.012 | 0.30 | 0.014 | 0.36 |
0.094 | 2.4 | 0.010 | 0.25 | 0.012 | 0.30 | 0.018 | 0.46 |
0.125 | 3.2 | 0.010 | 0.25 | 0.020 | 0.51 | 0.025 | 0.64 |
0.156 | 4.0 | 0.012 | 0.30 | 0.020 | 0.51 | 0.025 | 0.64 |
0.188 | 4.8 | 0.012 | 0.30 | 0.020 | 0.51 | 0.032 | 0.81 |
0.250 | 6.4 | 0.025 | 0.64 | 0.032 | 0.81 | 0.049 | 1.24 |
Y2 * Values | |||||||||
Cross Section C.S. | Ideal Compression e2 | Y2 * | |||||||
Thin | Medium | Heavy | |||||||
in | mm | in | mm | lb/in | DaN/cm | lb/in | DaN/cm | lb/in | DaN/cm |
0.035 | 0.9 | 0.006 | 0.15 | 457 | 80 | 1028 | 180 | 1485 | 260 |
0.063 | 1.6 | 0.012 | 0.30 | 571 | 100 | 799 | 140 | 1256 | 220 |
0.094 | 2.4 | 0.020 | 0.50 | 343 | 60 | 514 | 90 | 1313 | 230 |
0.125 | 3.2 | 0.026 | 0.65 | 343 | 60 | 1142 | 200 | 2056 | 360 |
0.156 | 4.0 | 0.031 | 0.80 | 171 | 30 | 857 | 150 | 1428 | 250 |
0.188 | 4.8 | 0.039 | 1.00 | 228 | 40 | 657 | 115 | 2113 | 370 |
0.250 | 6.4 | 0.051 | 1.30 | 799 | 140 | 1370 | 240 | 3026 | 530 |
Km Values | |
Material | Km |
321 SS | 1 |
Alloy 600 | 1.1 |
Alloy X750 | 1.3 |
Kd Values | |||||||||
Diameter | from : To : |
0.0" 0 0.75" 19 |
0.75" 19 1.2" 30 |
1.2" 30 2.0" 50 |
2" 50 3" 75 |
3" 75 6" 150 |
6" 150 10" 250 |
10" 250 18" 450 |
18"450 |
Kd Value | 1.4 | 1.3 | 1.2 | 1.1 | 1.0 | 0.9 | 0.8 | 0.8 |
Diameter / C.S. Guidelines | ||||||||
Cross Section | inch | 0.035" 0.9 |
0.063" 1.6 |
0.094" 2.4 |
0.125" 3.2 |
0.156" 4.0 |
0.188" 4.8 |
0.250" 6.4 |
mm | ||||||||
Diameter | from: inch | 0.250" | 0.500" | 1" | 2" | 3" | 4" | 5" |
from: mm | 6 | 12.5 | 25 | 50 | 75 | 100 | 125 | |
to : inch | 4" | 10" | 20" | 40" | 50" | 60" | 80" | |
to : mm | 100 | 250 | 500 | 1000 | 1250 | 1500 | 2000 |
Groove Assembly Types
Recommended Groove Dimensions
Notes : Please consult our engineering staff for cross sections larger than 0.250. Welds are finished flush with tube OD. Rings are blended within 0.125" of weld. Dimensions at blend zone are not more than 0.002"(per side) below adjacent surfaces. When restrained, the rings are round within diameter limits. (Consult our engineering staff for allowable tolerance for rings in the free state). Cross-section is subject to change during forming operation. (Consult our engineering staff for details). Calculating Groove Diameter: Internal Pressure: Groove OD (C) = Seal OD (A) + Clearance (CL) + [Maximum plating thickness x2] External Pressure: Groove ID (D) = Seal ID (B) - Clearance (CL) - [Maximum plating thickness x2] Example:
Calculation for U2312-03625 SEA (internal pressure)
Groove OD = 3.625 + 0.008 + [0.002 x2] = 3.637 (+0.04, -0.00)
Other Assembly types
A metal plate limiter can be added as a mechanical back-up that serves the same function as the machined groove. This allows the use of metal O-Rings on flat, raised or tongue and groove flange standards available on the market (ANSI, ASA, API, MSS SP 44, DIN etc...) usually without modification. The metal O-Ring can also be used on custom or shaped flanges.
Commercial O-Ring Specification
Example : U2312-03625SEA
The above example, U2312-03625SEA, indicates a type 321 stainless steel ORing, 3/32" (2.38mm) tube size, .012" (0.30mm) wall thickness, 3.625" (92.08mm) OD, self energized (ID) and .001-.002" (0.03/0.05mm) silver plating.